Pinholes, blade lines, a rough patch
Put a thin dab on just those places, let it dry, sand it flush. Nerolac's guide also allows touch-ups in patches on old, uneven walls. The rest of the wall stays at two coats.
New plaster takes two coats of putty. The first fills pores and trowel marks; the second gives the smooth white face the paint sits on. Both together stay under 1.5 mm. If the wall still shows dips after two coats, the answer is to level the wall, not to add a third coat.
Putty is a skin over the plaster, not a filler for a bad wall. Every coat goes on thin.
Spread thin with the blade, from the bottom up as Birla White suggests for WallCare. It fills pores, pinholes and trowel marks so the wall is nearly flat. Birla White is plain about it: keep it thin and even, don't try to cover big unevenness in one thick go.
Once coat 1 is dry and loose bits are knocked off, coat 2 goes on just as thin. It gives the smooth, white face. Birla White says the second coat should not be thicker than it needs to be: the 1.5 mm limit is for both coats added together.
After it dries overnight, a light sanding with fine paper, then every bit of dust wiped off. Primer goes over the putty before paint, never paint straight on putty. The full order is on our putty, primer, paint guide.
Can one coat do? Birla White's own WallCare FAQ says 1–2 finishing coats, depending on the wall. One coat is enough only where the surface is already smooth, such as a sound painted wall being repainted (putty on an old painted wall). On new cement plaster, plan for two.
The makers give different waiting times. These are brand figures for their own putty, not one rule. Where they differ, we go by the longer wait, and by touch: a putty coat that still feels cool is still wet.
| Step | Wait |
|---|---|
| Coat 1 to coat 2Birla White WallCare: at least 3 h · JK WallMaxX: 4–6 h · Asian Paints TruCare: 6–8 h | 3–6 h |
| Coat 2 to sanding and primerBirla White: "preferably overnight", 10–12 h | 10–12 h |
| Putty to paint, JK's figureJK WallMaxX page: let the wall dry 2–3 days before paint | 2–3 days |
| Water curing after puttyBirla White and Asian Paints: not needed | None |
| Mixed putty, use withinBirla White: 3–3.5 h. More on mixing putty | 3 h |
A third coat sounds like extra quality. On the wall, it is extra thickness, and thick putty cracks. Here is what to do instead, by what you see after coat 2.
Put a thin dab on just those places, let it dry, sand it flush. Nerolac's guide also allows touch-ups in patches on old, uneven walls. The rest of the wall stays at two coats.
Hold a straight patti on the wall. If the gap under it is more than putty's whole 1.5 mm, putty can't fill it. Birla White says WallCare "is not meant to be used as levelling material". Use its levelling putty as the first coat for shallow dips, or Levelplast for deeper ones, then WallCare.
A thick layer dries on the outside first while the inside is still wet, and it cracks (Birla White's list of putty mistakes). Whiteness and strength come from primer and paint, not more putty. If it has happened: paint lifting after putty.
Two makers give the same limit: Birla White for WallCare, and Asian Paints for TruCare, 1.5 mm for both coats together. Neither gives a separate figure for each coat. In practice the first coat carries a little more, because it fills the pores; the second is a thin skim.
Thick putty dries on the face first while the inside stays wet. The face then cracks, and paint over it flakes. Birla White lists "applying a very thick coat" among its common putty mistakes.
Two quick tests. The straight-edge test (above). And the bag count: two thin coats use a known amount of putty per square foot, so an order far above it means thick coats. Try it in check the bags below.
All three makers say the same thing. Asian Paints' sheet says not to use its putty to fill cracks. JK says fill cracks and holes with a cement-sand mix or filler first. Birla White says significant cracks must be repaired before putty.
Shrinkage lines thinner than a hair. Brush the dust out of them, wet the wall, and the two coats of putty fill them in the normal way.
Open it into a V, dust it, fill it with crack filler or a cement-sand mortar (SBR in the mix helps it grip), let it dry, then putty. Which filler for which width: putty vs crack filler · cracks before painting.
Cracks from window and door corners, through the wall, or ones that reopen after filling, have a cause that putty won't stop. Send photos on WhatsApp and we'll check them with you. How to tell: structural crack or plaster crack.
Birla White itself says putty is not mandatory for every paint system. It decides how the paint looks, so it matters most where you'll see it. The full comparison, with what skipping saves: putty or no putty.
Put in your room. Two thin coats on smooth plaster use a known amount. An order far above it means coats are going on thick, or a third coat is planned. Ask why before you buy.
WallCare packs: 1, 5, 20, 40 kg. Today's price: putty rates. Whole house: how many bags of putty.
Prices are from our latest bill and change often. Please confirm today's rate on WhatsApp or call before buying.
Birla White WallCare puttyThe two coats, inside walls · 1, 5, 20, 40 kg₹ 481per 20 kg Birla White Lemon puttyWallCare with lemon fragrance · 20 kg₹ 435per 20 kg Birla White Waterproof puttyDamp-prone and outside walls · 40 kg₹ 1,405per 40 kgBirla White's levelling putty (WallCare MF) and any pack size not on the shelf: we order it for you; ask on WhatsApp for the time it takes. Today's prices: putty rates.
Two thin coats on new plaster. The first fills pores and trowel marks, the second gives the smooth white face. Birla White, JK and Asian Paints all describe a two-coat job, and Birla White and Asian Paints cap both coats together at 1.5 mm.
Almost never as a full coat. Pinholes or blade marks left after coat two are filled as spot patches. Dips and waves need levelling first (Birla White's levelling putty, or Levelplast), then the usual two coats. A third full coat pushes the putty past 1.5 mm, and thick putty cracks.
On new cement plaster, no. On a smooth surface, such as a sound old painted wall that has been sanded, one skim coat can do; Birla White's FAQ allows 1–2 finishing coats depending on the wall. See putty on an old painted wall.
Birla White and Asian Paints give the limit for both coats together, 1.5 mm, not for each coat. The first coat takes a little more because it fills the pores; the second is a thin skim. If the wall needs more than that, it needs levelling, not putty.
Yes, lightly. Between coats, a wet sponge, the putty blade or fine waterproof emery knocks off loose bits (Birla White). After the last coat, sand gently with fine paper: the Birla Opus sheet names No. 320, and Birla White's WallCare guide says no coarser than 500. Coarse paper damages the putty. Then wipe off all the dust before primer.
Only hairline cracks. Asian Paints' sheet says not to use putty to fill cracks, JK says to fill cracks with a cement-sand mix or filler first, and Birla White says significant cracks must be repaired before putty. A crack that is diagonal, wider at one end or keeps coming back needs its cause found; send photos on WhatsApp and we'll check them with you.
For a smooth emulsion finish on new plaster, yes. For a cement paint or distemper wall on a budget, no; the paint goes on primed plaster. Birla White itself says putty is not mandatory for every paint system. More in putty or no putty.
Birla White says at least 3 hours for WallCare, JK says 4–6 hours for its putty, Asian Paints 6–8 hours for TruCare. After the last coat, overnight (10–12 hours, Birla White) before sanding and primer. In humid weather, longer. Details: putty drying time.
No. Birla White and Asian Paints both say their putty needs no water curing. The wall is wetted before the first coat, without water running down it.
Paint Engineer at our Reva Road store, Muzaffarpur. Every number on this page was checked against the maker's own page or sheet on 12 Nov 2026. Where the makers give different figures, the page shows each one with its name.