The short answer

Cement is cheaper and still works for small ceramic tiles on a new floor. Everything bigger, denser, higher up or outside needs adhesive.

  • Cement OK300 × 300 ceramic floor, new level floor, full bed with slurry
  • AdhesiveWall tiles · 600 × 600 vitrified and bigger · planks · over old tiles · outside
  • NeverCement mixed into adhesive, or dabs of adhesive in place of a full bed

The reason is the tile, not the brand: cement grips by soaking into the tile's back, and vitrified tiles hardly soak up anything.

≤ 0.5%
Water a vitrified tile takes inA ceramic wall tile takes in over 10%. That is what cement holds on to.
20 → 6
mm of bed under the tileCement-sand bed against an average adhesive bed. The floor ends up 14 mm lower.
24 h
Then walk on adhesiveTX2 and Vitribind data sheets. No soaking the tiles, no water curing.
The two beds, drawn to one scale
Cement-sand bed and adhesive bed compared in section Top: tiles on a 20 mm cement-sand bed with cement slurry, with air pockets under the tiles where the mortar shrank, so a tile sounds hollow when tapped. The floor rises about 28 mm. Bottom: a tile on a 6 mm combed adhesive bed pressed flat with full contact, and ridges of adhesive waiting for the next tile. The floor rises about 14 mm. Cement-sand bed what most masons here do · 1 cement : 4 sand tileslab 20 mm Air pockets where the mortar shrank: tap the tile and it sounds hollow Tiles soaked, cement slurry on the bed floor goes up about 28 mm with an 8 mm tile Adhesive bed TileStix, combed with a notched trowel next tile: press and slide tileslab 6 mm Ridges pressed flat: full contact tile laid dry, no soaking, no slurry Floor goes up about 14 mm
Bed and tile thicknesses to one scale. Cement bed: 20 mm of 1:4 mortar with grey cement slurry, as in CPWD-style tender items. Adhesive: 6 mm, the average those items allow; TileStix allows 3 to 12 mm.
Why big tiles go hollow

Why cement lets go of vitrified tiles

Cement-sand worked for decades because tiles used to be small, thick and porous. Today's tiles are none of those.

1Cement grips by soaking in

Wet cement paste is drawn into the pores on the back of a ceramic tile and sets there. A vitrified tile is pressed and fired until it takes in 0.5% water or less. The paste only touches the surface, so the bond is weak from day one.

2A thick bed shrinks

A 20 mm bed holds a lot of water. As it dries and sets it shrinks, and small gaps open under the tile. A 300 mm tile bridges them. A 600 mm or 1200 mm tile flexes over them when you walk, and the corners crack or the tile pops.

3Walls and old tiles are worse

On a wall, wet mortar is heavy and each row can slide before it sets. On old tiles, the glaze takes in nothing at all. Adhesive is made for both: Birla White calls Intero Grip+ sag resistant and allows it for tile-on-tile work.

How cement holds a ceramic tile and fails to hold a vitrified tile Magnified view. Top: a ceramic tile body full of pores, with cement paste reaching up into them like roots. Bottom: a dense vitrified tile body with almost no pores; the cement paste meets a flat surface and a thin gap opens along it. Ceramic wall tile takes in over 10% of its weight in water cement paste The paste is drawn into the pores and sets there, like roots. Vitrified tile takes in 0.5% or less cement paste Nothing soaks in. The cement only touches the surface and lets go when the bed shrinks or the slab moves.
Magnified, not to scale. Water absorption limits: IS 15622 tile groups (vitrified 0.5% or less; ceramic wall tiles over 10%). Adhesive holds by polymer and fine cement, not by soaking in.

When a cement bed is fine

We are not against cement. It does this job well when:

  • the tiles are small and porous: our 300 × 300 ceramic floor tiles;
  • the floor is new concrete, so the 28 mm rise doesn't matter;
  • the mason lays a full bed and pours slurry on it, and taps every tile down;
  • the floor is kept damp and off-limits while the mortar cures (usual practice: a few days).

A cement bed also levels a rough or sloping slab in one go. Adhesive cannot fill dips: TileStix is laid 3 to 12 mm thick, so a bad floor gets a screed first. If your slab is uneven, that is part of the cost. See what each costs.

For each tile we sell

What we tell people at the counter, tile by tile

Birla White sets a tile type and a largest size for each TileStix grade. Here is each tile on our shelf with the method we'd use.

300 × 300 floor

Ceramic · bathroom, kitchen, store room floors
Cement bed OKor TX2 · 3 mm

The one tile a cement bed still suits: small and porous, on a new floor. Insist on a full bed and slurry, not dabs. If the floor is already level, TX2 at 3 mm is quicker and keeps the floor lower at the door.

300 × 450 wall

Ceramic · bathroom and kitchen walls
Cement: rows slipTX2 · 3 mmOn our shelf

Masons here fix these on wet mortar with slurry, tiles soaked. It holds on porous tiles, but it is heavy and rows sag before it sets. TX2 is made for this: ceramic up to 450 × 450 mm, inside, sag resistant.

Tiles go on cement plaster, never on putty. Putty is only for the wall above the tiles.

600 × 600 vitrified

Glazed vitrified, double charge, soluble salt · rooms and halls
Cement: goes hollowVitribind · 6 mmWe order it

Big and dense: exactly the tile that goes hollow on a cement bed. Birla White's grade for vitrified up to 600 × 600 mm is Vitribind. TX2 is not for vitrified tiles, whatever the mason says.

600 × 1200 and 200 × 1200 planks

Large slabs and wooden-look planks
Cement: noExtero · about 8 mmWe order it

Long tiles are past Vitribind's 600 mm limit, so use Extero (up to 1200 × 1200 mm). Spread adhesive on the tile's back as well as the floor, so the ends are not left hollow (usual practice for 1200 mm tiles).

400 × 400 outdoor

Anti-skid · porch, terrace, parking, ramps
Cement: cracksExtero · 6 mmWe order it

Sun on a terrace makes tiles grow and shrink every day. Birla White asks for Extero outside because it gives with that movement, and says gaps between tiles are compulsory outside: never butt-joint them.

New tiles over old tiles

Re-doing a floor or bathroom without breaking
Cement: noTX2 or Vitribind

A glaze takes in nothing, and 20 mm of mortar would jam the doors. Birla White allows TX2 and Vitribind for tile-on-tile inside: TX2 for ceramic, Vitribind for vitrified. Old tiles must be sound (no hollow ones), clean and grease-free.

Tile drawings to one scale: the dashed square is 1200 × 1200 mm, the largest tile Extero takes. Limits from Birla White's TileStix pages: Intero Grip+ ceramic up to 450 × 450 mm inside; Vitribind up to 600 × 600 mm; Extero up to 1200 × 1200 mm, inside and outside.

What each costs

Side by side, and the material for your floor

On material alone, adhesive costs more than cement and sand for a 600 × 600 floor. On a 3 mm bed for small tiles the gap is small. What you buy with the difference is a floor that doesn't need re-laying.

Cement-sand bedTileStix adhesive
Bed under the tile20 mm floor, 12 mm wallCPWD-style tender items3–12 mm6 mm average on floors
Floor goes up bywith an 8 mm tileabout 28 mmabout 14 mm
Weight on the slababout 40 kg per sq musual figure for 20 mm of mortarabout 10 kg per sq mwet density 1.6–1.8 kg/L (data sheet)
Soak the tiles firstYesNo
Vitrified tilesWeak gripVitribind or Extero
Wall tilesHeavy, rows slipTX2, sag resistant
Over old tilesNoTX2 or Vitribind
OutsideCracks in sun and rainExtero, with gaps
Fills dips in the slabYes, in the same bedNo, screed first
Walk on itAfter curing with waterusual practice: a few days24 hoursExtero: heavy loads after 28 days
Material, 100 sq ft floorabout 2 bags cement + 7 cft balu2 bags (3 mm) to 5 bags (8 mm)
Material priceAsk rateAsk rate

Your floor or wall

—

Material for each way

Cement-sand bed

Prices are from our latest bill and change often. Please confirm today's rate on WhatsApp or call before buying.

UltraTech PPC cement
——Ask today's rate per 50 kg bag
Balu (coarse sand)—For the mortar only. Grout extra.Ask today's rate per cft
Adhesive
———Ask rate per 20 kg bag
Material totalsAsk rate
Ask today's price on WhatsApp

Cement way: 1:4 mortar 20 mm thick on floors (1:3, 12 mm on walls), dry volume taken as 1.27 times wet, plus 3.3 kg of cement slurry per sq m. Adhesive: bed × area × the powder per litre of wet mix from each TileStix data sheet; bags are for the middle of the range, so add one if the floor is rough. Labour is separate and paid to your mistri: tile laying rates. Tiles, grout and boxes: tiles calculator.

Where each one fails

Cement fails in three ways. Adhesive, laid badly, in three more.

Adhesive is not magic. Each picture shows the bed on the left (red is the fault) and what you see on the floor or wall later.

AIR POCKETS
Cement bed

Vitrified tiles on a cement bed

You see: a hollow "dhab-dhab" sound, then cracked corners

The bed shrank and the dense tile never gripped. Tap every tile with a coin: a hollow one will fail first. Fix: hollow and lifting tiles.

NO GAP
Cement bed

Tiles pop up in a row

You see: two tiles lift into a ridge, often in May–June

Tiles laid tight with no gaps, on a weak bed, have nowhere to grow in the heat. Leave joints and edge gaps at walls whatever bed you use; outside, Birla White says gaps are compulsory.

WET, HEAVY
Cement bed

Wall tiles that slide and bulge

You see: wavy rows, wide gaps, hollow tiles at eye level

Wet mortar is heavy and slow to set, so each row creeps down. TX2 is sag resistant and allowed up to 3 m high on walls. Over that height, ask Birla White's team.

DOT FIXING emptyunder here
Adhesive

Five dabs in place of a full bed

You see: corners crack or rock when stepped on

Dabs save adhesive and leave most of the tile in the air. Comb the whole area with a notched trowel and press the tile in until it sits on all of it.

SKIN FORMED 20 MIN
Adhesive

Adhesive spread too far ahead

You see: a tile that lifts off clean, back still shiny

TX2 and Vitribind stay open for about 20 minutes, Extero about 30, at 25°C. Less in Bihar's summer heat. Spread only what you can tile in that time; touch it, and if it doesn't stick to your finger, scrape it off.

JUST WATER 20 KG + CEMENT no cement · no extra water
Adhesive

Cement "for strength", or extra water

You see: weak, powdery bed; tiles loosen in months

The bag already holds cement. Birla White says just add water, 4.8–5.2 L per 20 kg of TX2. Mix only what you can use in 2 hours, and never add water again to a stiffened mix.

What masons here say

Six things you'll hear at site, and the answer

Most masons in Muzaffarpur learnt on cement beds and are good at them. These are the lines that come up when the tile is new to them.

Cement is stronger than this powder

The powder is cement too, with polymers and graded sand. TX2 is tested to IS 15477 Type 1T; Extero to Type 3T and the European C2TE, a higher class. A thick bed is not a strong bond.

Put a little cement in the adhesive, it grips better

No. The bag already holds cement in a tested mix. Birla White: just add water. Roff: no need to add cement.

Soak the tiles first

Only for a cement bed. With adhesive, lay tiles clean and dry. A dripping tile waters down the adhesive under it.

Slurry on top is as good as adhesive

Slurry helps the bed stick, but the bed still shrinks and the vitrified tile still takes in almost nothing. That is the gap that sounds hollow later.

TX2 works for every tile

Birla White's own limit for TX2 is ceramic up to 450 × 450 mm, inside. Vitrified needs Vitribind or Extero. Bring us the tile size and we'll give the right bag.

Adhesive work costs more labour

Ask for both rates in writing. Adhesive work skips the tile soaking and the slurry, but needs a level base and a notched trowel. See tile laying rates.

Questions people ask us

Short answers

Is tile adhesive better than cement?

For vitrified tiles, wall tiles, tiles over old tiles and anything outside, yes. Cement grips by soaking into the back of the tile, and vitrified tiles take in almost no water. For 300 × 300 ceramic floor tiles on a new, level floor, a full cement bed with slurry still does the job if it is laid well.

Can I add cement to tile adhesive?

No. It already contains cement. Birla White says TileStix needs only water (4.8–5.2 L per 20 kg of Intero Grip+), and Roff says there is no need to add cement. Extra cement or extra water changes the mix the adhesive was tested at.

How many bags of tile adhesive for 100 sq ft?

About 2 bags of 20 kg on a 3 mm bed (small ceramic), about 4 on a 6 mm bed (600 × 600 vitrified) and about 5 on an 8 mm bed (600 × 1200 and planks). We worked this out from each TileStix data sheet's mixing ratio and wet density. Orientbell gives 25–30 sq ft per 20 kg bag for its own adhesive, which matches a 6 mm bed. More detail: how much tile adhesive.

Can your TileStix TX2 fix vitrified tiles?

No. Birla White says Intero Grip+ is for ceramic and semi-vitrified tiles up to 450 × 450 mm, inside, and that vitrified tiles need Vitribind or above. Vitribind goes up to 600 × 600 mm; Extero up to 1200 × 1200 mm, inside and outside. We order both for you.

Do tiles need soaking with adhesive?

No. Soaking is a cement-bed habit: it stops a porous tile pulling water out of the mortar. Adhesive holds its own water; Asian Paints lists no pre-soaking among adhesive's advantages. Lay tiles clean, with the dust wiped off the back.

When can we walk on it and grout?

After 24 hours for Intero Grip+ and Vitribind. Extero takes foot traffic after 24 hours and heavy loads after 28 days. These are at 25°C; allow longer in cold, damp weather. Grout with TileLynk once the tiles are set.

Is tile adhesive waterproof?

It is water resistant and made for wet areas, but it is not a waterproofing layer. On a bathroom floor, waterproof the base first (we use Seal & Dry SBR in the base coat and Hi-Flex under the tiles), then tile with adhesive. See bathroom waterproofing.

Can I lay new tiles on old tiles with cement?

No. Glazed tiles take in nothing, so cement has nothing to grip, and the floor rises nearly 3 cm. Birla White allows Intero Grip+ and Vitribind for tile-on-tile inside, over old tiles that are sound and clean. Full steps: tiles on old tiles. Other questions: adhesive and grout FAQ.

Mr Mustafaa
Paint Engineer, Tashya Ventures

Paint Engineer at our Reva Road store, Muzaffarpur, who also answers our tile, putty and waterproofing questions. Every figure on this page was checked against the maker's own data sheet on 12 Nov 2026. Where a maker's pages disagree, the page says so and gives the safer choice.

Where the numbers come from

  1. Birla White, TileStix Intero Grip+ page (FAQ) and technical data sheet: ceramic and semi-vitrified up to 450 × 450 mm, inside; vitrified needs Vitribind or above; outside needs Extero; tile-on-tile allowed; 4.8–5.2 L water per 20 kg; mixing ratio 0.24–0.26; wet density 1.60–1.80 kg/L; open time about 20 min; pot life 2 h; 24 h to heavy traffic; bed 3–12 mm; IS 15477:2019 Type 1T.
  2. Birla White, TileStix Vitribind page and data sheet: vitrified, porcelain and ceramic up to 600 × 600 mm; walls up to 3 m; 5.2–5.6 L water per 20 kg; ratio 0.25–0.27; IS 15477 Type 2T. One FAQ answer lists outside floors, another sends all outside work to Extero; we follow the safer one.
  3. Birla White, TileStix Extero page and data sheet: up to 1200 × 1200 mm, inside and outside; spacing between tiles compulsory outside; 6–6.4 L water per 20 kg; ratio 0.30–0.32; wet density 1.55–1.75 kg/L; open time 30 min; foot traffic 24 h, heavy traffic 28 days; IS 15477 Type 3T, EN 12004 C2TE.
  4. Roff, NCA product page (FAQ): adhesive already has cement, no need to add more.
  5. Asian Paints, tile adhesives against cement: cement beds shrink and leave hollows; adhesive needs no pre-soaking.
  6. Orientbell, FAQ: 25–30 sq ft per 20 kg bag of its adhesive.
  7. CPWD-style tender items, e.g. Prasar Bharati (Doordarshan Kendra Chennai, 2022) and SBI premises BOQs: vitrified tiles on a 20 mm bed of 1:4 cement mortar with grey cement slurry at 3.3 kg/sq m; skirting on a 12 mm bed of 1:3; or tiles laid with adhesive to IS 15477 in an average 6 mm thickness.
  8. IS 15622 tile groups: vitrified tiles take in 0.5% water or less; ceramic wall tiles over 10%.

Usual practice, not from a maker's sheet: dry mortar volume 1.27 × wet; mortar weight about 2,000 kg per cubic metre; 8 mm bed and back-buttering for 1200 mm tiles; a few days of curing before walking on a cement bed.

Send us your tile and room size

We'll tell you cement or adhesive, which TileStix bag, and how many, with today's price, on WhatsApp.

TASHYABUILDING SOLUTIONS · MUZAFFARPUR
WhatsApp 90310 74624tashyaventures.com