हिंदी Call90310 74624
Home›Waterproofing›Bathroom
Waterproofing guide · bathroom

Bathroom waterproofing: the sunken floor, the walls, the pipes, all before the tiles

The short answer
  1. Plumbing done and tested
  2. Pipes packed, gola at corners
  3. Coat × 2 in the sunk
  4. 48 h water test
  5. Filling, sloped screed
  6. Coat × 2 again
  7. Tiles

A bathroom gets two waterproof layers: one inside the sunken floor before it is filled, and one just under the tiles. Most leaks into the room below come through the gaps: round a pipe, at the floor trap, or where the floor meets the wall. The flat middle of the floor rarely leaks. Once the tiles are on, all of this is buried, so it has to be right first time.

2 + 2
CoatsTwo inside the sunk, two under the tiles, each laid across the one before.
48 h
Water test50 mm of water stays on the coated floor for 48 hours before anything covers it (Birla White).
~4 wk
Before the first bathCuring and testing by the makers' sheets. This is not a two-day job.
A sunken bathroom floor, cut open
Cross-section of a waterproofed sunken bathroom floor The concrete slab is dropped below the next room's floor. A pipe passes through the slab in a packed sleeve. Rounded mortar fillets sit in the corners. A red waterproof coat lines the sunk and runs up the wall. Over it are a protection plaster, brick filling, a screed sloped to the floor trap, a second red coat that runs up the wall, and the floor and wall tiles. The coat goes up the wall: 1 ft on every wall about 4 ft where you bathe to the shower head, with a shower next room sunk depth 9 in to 1½ ft (usual; go by your drawing) ceiling of the room below 1 2 3 4 5 6 7 8 9 1 2 3 4 5 6 7 8 9 Slab · WP+200 in the concrete, 200 ml per bag Pipe sleeve · packed solid with SBR mortar Gola · rounded mortar in every corner, ~2 in Coat × 2 · Hi-Flex or Seep Blocker 2K, in the sunk Protection plaster · so filling can't cut the coat Filling · brick pieces in lean mortar Screed · sloped down to the floor trap Coat × 2 again · floor, trap neck, up the walls Tiles · on TileStix, joints in TileLynk Water test, 50 mm for 48 h on the bare slab, on the coat (4), and before the tiles
Not to scale: the coats are far thinner than drawn. Red is the waterproof coat. Sunk depth and filling are usual local practice; the coats, gola and water test follow the UltraTech and Birla White sheets.
Which parts get the coat

The whole floor, a foot up every wall, and the wall you bathe at

The makers give different minimums for the walls. Dr. Fixit says 20 cm, Birla White says at least 300 mm and higher in the shower. We go with 1 ft, the higher of the two.

A 6 by 8 ft bathroom opened out flat, with the coated areas marked The floor is in the middle and the four walls are folded out around it. The whole floor is coated, and a 1 ft band runs up every wall. The tap wall is coated to 4 ft and, with a shower, on up to about 7 ft. A 2 ft strip on each side wall next to the tap wall is coated to the same height. Rings mark the floor trap and the WC pipe. The coat runs under the door frame. DOOR FLOOR 6 × 8 ft all of it, twice WALL AT THE TAP basin WC 4 ft bucket bath ~7 ft with a shower coated carry on up ifthere's a shower seal round it 1 ft up every wall Dr. Fixit 20 cm, Birla White 300 mm; we use the higher one. Under the door frame carry the coat across the threshold, so water can't creep out under it. Opened out flat: fold the four walls up round the floor.
Drawn for a 6 × 8 ft bathroom, 1 square = 1 ft. Wall heights are usual practice. The 20 cm and 300 mm minimums are from Dr. Fixit's FAQ and Birla White's bathroom guide.

FloorTwice: in the sunk and under the tiles

The first layer lines the bare sunken slab and its sides before the filling goes in. The second goes on the sloped screed just under the tiles. Dr. Fixit and Birla White both put the sunk coat on before filling, because once it's filled nobody can get at it.

1 ftEvery wall, all round

The joint between floor and wall is where a floor coat most often fails. Carry the coat up over the gola and at least 1 ft up the plaster, behind the WC and basin too.

4 ftThe wall you bathe at

With a bucket and mug, water splashes to about 4 ft on the tap wall and about 2 ft along the side walls next to it (usual practice). With a shower, take it up to the shower head, about 7 ft, or to the top of the tiles.

RingsEvery pipe and the floor trap

Every pipe that passes through the slab or the sunk wall gets its gap packed solid, then the coat is carried a little way up the pipe. The second coat goes down into the neck of the floor trap. Birla White's warranty doesn't cover leaks from the trap or untreated tile joints, which shows how often these spots fail.

DoorUnder the threshold

Water creeps along the screed and out under the door frame into the next room, so the coat runs across the threshold too (usual practice).

The same idea works for a kitchen: the floor of the washing area and the sink wall up to counter height. Dr. Fixit says a kitchen usually has less standing water, so the treatment can be lighter: kitchen waterproofing.

Step by step

A new bathroom, from bare sunk to tiles

Thirteen steps in three stages. Red steps are work and blue steps are water tests. The waits come from the UltraTech and Birla White sheets. Where the two differ, we give the longer wait.

Before step 1: all plumbing and sanitary work finished and tested (Birla White makes this a condition). Have the plumber fill the supply pipes and leave them under pressure for a day to check for leaks (usual practice). New concrete and plaster should have cured for 28 days (Birla White).

Stage 1 · Inside the sunk before any filling

  1. 1

    Slab with WP+200

    At dhalai, mix WP+200 into the concrete at 200 ml per 50 kg bag of cement, in half the mixing water (UltraTech). If the slab is already cast, go to step 2.

    at casting
  2. 2

    Clean and repair

    Chip off loose bits and fill honeycombed patches. Birla White says to fill cracks under 3 mm with a crack filler and repair wider ones with polymer mortar. Wet the slab just before the next step, with no water left standing on it.

    same day
  3. 3

    Pack every pipe sleeve

    Rough up the pipe with sandpaper (usual practice). Brush a cement slurry made with Seal & Dry SBR onto the pipe and the concrete. Then pack the gap solid with mortar made with SBR and WP+200, and mix as printed on the SBR pack. Birla White's sheet uses a non-shrink grout with an epoxy seal on top instead. Either way, the gap must be filled solid, not just smeared over.

    cure a few days
  4. 4

    Gola in every corner

    Make a rounded fillet about 50 × 50 mm (2 in) where the sunk floor meets its walls. Birla White makes it with SBR polymer mortar over an SBR bond coat and keeps it damp for 3–4 days. It also asks for glass-fibre mesh in the first coat over the gola. We can order the mesh for you.

    3–4 days damp
  5. 5

    Water test the bare slab

    Block the outlets and fill 50 mm of water for 48 hours (Birla White). If the ceiling below shows a patch now, fixing the slab is cheap. After the floor is tiled, it isn't.

    48 h
  6. 6

    Coat × 2, crosswise

    Hi-Flex: two coats, 0.6–0.7 mm each, at least 8 hours apart, the second at right angles to the first (UltraTech). Or Seep Blocker 2K: add 2 parts powder to 1 part liquid, with no water, let it stand 5 minutes, then brush on. Leave 6–8 hours between coats (Birla White). Cover the floor, the sunk walls, the gola and the pipe collars, and carry the coat about a foot up the room walls.

    6–8 h · Hi-Flex ≥ 8 h
  7. 7

    Cure it

    Seep Blocker 2K: let it air-dry for 3–6 hours with no water on it. Then keep it damp for 2–3 days by spraying or with wet sacking, and let it air-dry for 3–4 days before water stands on it (Birla White). Hi-Flex: cure as printed on the pack. Don't apply either above 35 °C surface heat or in the afternoon sun (Birla White).

    about a week
  8. 8

    Water test the coat

    About 7 days after coating, fill 50 mm of water for 48 hours with the outlets closed (Birla White). Chalk the water level on the wall and check the ceiling below twice a day. Drain it without scratching the coat.

    48 h

Stage 2 · Protect and fill the coat is buried for good

  1. 9

    Protection plaster

    Birla White's sheet: 2–3 mm of Levelplast, or a spatterdash of cement, SBR and coarse sand at 1:1:1.5. After 24–48 hours, add 12–15 mm of 1:4 cement plaster, then cure it 7 days. UltraTech likewise recommends a screed or plaster over Hi-Flex. This layer stops broken brick and the mason's tools from cutting the coat.

    7 days
  2. 10

    Fill the sunk

    The usual practice here is broken brick set in a lean cement mortar, packed firmly round the trap and pipes. Don't use loose sand or site rubbish: if water ever gets in, they soak it up and hold it like a sponge.

    a few days
  3. 11

    Screed sloped to the trap

    Lay 1:4 mortar with WP+200, falling towards the floor trap. Set the top of the trap so the finished tiles run down into it. A fall of about ½ inch over 4 ft (1 in 100) is usual practice. If drain pipes run on the floor, Birla White wants the screed at least 20 mm thick over them.

    keep damp

Stage 3 · Under the tiles the second line of defence

  1. 12

    Coat × 2 again, then test

    On the dry screed, into the neck of the floor trap, 1 ft up every wall, and up the wall you bathe at. While the second coat is still wet, throw dry coarse sand onto it so the tile adhesive has something to grip (usual practice). Water-test the floor once more, overnight or for a day (usual practice).

    cure, then test
  2. 13

    Tiles

    Fix the tiles with TileStix Intero Grip+ (TX2), which Birla White rates for ceramic tiles up to 450 × 450 mm indoors. That covers our 300 × 300 floor and 300 × 450 wall tiles. Fill the joints with TileLynk, and seal the joint round the trap and every pipe outlet. You can walk on the tiles after 24 hours (Birla White). Never put putty under tiles.

    walk after 24 h

Which tile won't slip: bathroom floor tiles. Laying them level and tight: how tiles are laid. Want us to check the work? Send photos on WhatsApp before the sunk is filled and before the tiles go on, and we will look at them with you.

How long before the first bath

About four weeks, done properly

This counts from a cured slab with the plumbing done. Most of the time goes on curing and water tests, not on work. A thekedar who promises the bathroom in three days is skipping the curing and the tests.

StageWait
Gola, kept dampBirla White sheet3–4 days
Water test, bare slab50 mm of water (Birla White)48 h
Coat 1 to coat 2Seep Blocker 2K: 6–8 h (Birla White sheet; its blog says 5–6 h) · Hi-Flex: at least 8 h (UltraTech)6–8 h
Curing the coatSeep Blocker 2K: 2–3 days damp, then 3–4 days dry~7 days
Water test, coated sunk50 mm of water (Birla White)48 h
Protection plaster cureBirla White: mist spray 3 times a day7 days
Filling, screed, second coatUsual practice; coat cured as per its pack4–6 days
Tiles to walkingTileStix TX2 (Birla White)24 h
From bare sunk to first bath~4 weeks
Where Birla White's own sheet doesn't add up. It asks for the water test about 7 days after the last coat, but also for the protection plaster within 3–5 days of the last coat. You can't do both. We do the water test first, because a coat that leaks is worth nothing however well it is protected, and then lay the protection plaster straight away. If you plan to claim the warranty, ask Birla White (1800-111-717) which date they want.
Before you count on a warranty. Our 3 kg Seep Blocker 2K carries Birla White's 3-year warranty only if at least 12 kg is used on one surface, the warranty is registered within 30 days of purchase, and the steps above are followed. The warranty excludes leaks from floor traps, untreated tile joints and plumbing. Keep the bill and the batch number from the pack.
Monsoon and summer. Damp air slows every cure. In May and June, Birla White asks you not to coat when the surface is above 35 °C, so coat in the morning, not the afternoon.
What goes wrong

Six ways a bathroom ends up leaking into the room below

Each picture shows the fault on the left (red marks the mistake) and what you see months later on the right. Dr. Fixit's FAQ makes the same point: a good product is usually let down by how it was applied.

NOT UP THE WALL

Coat stops at the floor line

You see: a damp band along the bottom of the next room's wall

Water runs into the floor-wall joint and through the wall. Take the coat over the gola and at least 1 ft up every wall.

GAP LEFT OPEN

Pipe sleeve smeared, not packed

You see: a round stain on the ceiling below, round the pipe

The commonest bathroom leak. Pack the gap solid with SBR mortar, then carry the coat up the pipe. This is step 3.

NO PROTECTION

Filling thrown straight on the coat

You see: drips from the middle of the ceiling below

Sharp brick and a mason's tools cut a bare coat. Birla White puts a 12–15 mm protection plaster over the coat first. This is step 9.

trap set high WRONG SLOPE

No slope, or the trap set too high

You see: water standing in a corner, joints turning black

Standing water finds every weak joint. Slope the screed down to the trap and set the trap's top below the tiles. This is step 11.

50 mm TEST SKIPPED

No water test before covering

You see: the leak after the tiles are on, then a broken floor

Forty-eight hours of water costs nothing. Finding the leak after tiling costs the whole floor. These are steps 5 and 8.

LEAK NOT STOPPED

Putty and paint on the wall outside

You see: the stain is back within weeks

Even waterproof putty does not stop an active leak. Stop the water in the bathroom first, let the wall dry fully, then waterproof putty, primer and paint.

An old bathroom that leaks

Fix it without breaking, or break the floor?

Birla White's post on old bathrooms coats the existing walls and floor with Seep Blocker 2K without a full renovation. It doesn't say when that isn't enough. Dr. Fixit warns that re-grouting alone rarely stops an existing leak. Here is how we tell the cases apart. For the full repair guide, see bathroom water reaching the room below.

First, the 2-day test: pipe or floor?

Don't use the bathroom for two days, but leave the water supply on. Mark the edge of the stain below with a pencil.

Stain still growing: a supply pipe is leaking under pressure. That's a plumber's job, not a coating: leaking pipe joint.
Stain drying: the water comes from use, through the joints, the trap or the floor. Read on.

Joints open, tiles firm

Leak shows only after bathing; tiles don't sound hollow when tapped
Rake out jointsTileLynkSBR round trap
  • Rake out the old grout and re-fill every floor joint and the lowest wall rows with TileLynk.
  • Chip out round the floor trap and pipe outlets, then reset them in SBR mortar.
Check the ceiling below again after two weeks of normal use. If the stain is still there, go to the last card.

Wall above the tiles is damp

Plain plaster above the dado, or the shower wall with no tiles
Stop the water firstSeep Blocker 2K × 2Putty, primer, paint

Next room's wall is wet at the bottom

A tide mark at floor level on the far side of the bathroom wall
Floor-wall jointDoor threshold
  • Water is leaving at the floor-wall joint or under the door frame. Re-grout the bottom row and the corner joints, and seal the threshold.
  • Let the outside wall dry fully before any putty or paint. Test it by touch and colour; it usually takes a few weeks after the leak is fixed.

Time to break the floor

Stain stays after re-grouting, floor sounds hollow, trap or pipe in the sunk broken
Floor tiles upEmpty the sunkSteps 2–13
  • The sunk is full of water and no surface coat will dry it. Lift the floor tiles, dig out the wet filling, and let the sunk dry.
  • Then follow steps 2 to 13 above. Dry wall tiles can usually stay; coat the bottom 1 ft once the floor tiles are off.
How much to buy

Quantities for your bathroom (a 6 × 8 ft one to start)

Put in your bathroom's size. Coat areas include the sunk sides, 1 ft up every wall and the wall you bathe at, for both layers. Coverage comes from the makers' sheets, read the safe way.

Area to coat: — sq ft (sunk layer — + under-tile layer —)

Wet wall: the tap wall plus about 2 ft along each side wall. A 6 ft tap wall with two 2 ft returns is 10 ft.

Your list

Weather Pro Hi-Flex, 2 coats × 2 layers—1 kg covers 14–15 sq ft for one coat (UltraTech), so two coats take double—
UltraTech cement, protection plaster + screed—1:4 mortar: 15 mm in the sunk, about 40 mm average screed with the slope (usual practice). Filling mortar not included.—
Weather Pro WP+200—200 ml per 50 kg bag of cement (UltraTech)—
Seal & Dry SBR, gola and pipe sleeves1 kgMix with cement as printed on the pack. A bigger bathroom or many pipes may need the 20 kg pack.Buy: 1 × 1 kg · Ask rate
Material totalAsk rate
Send this list on WhatsApp

Prices are filled in from today's rate. Tiles, TileStix and TileLynk: tile calculator. Roof, tank or any other job: waterproofing calculator. Glass-fibre mesh or non-shrink grout: we can order it for you; ask on WhatsApp how long it takes.

Questions people ask us

Short answers

Which is the best waterproofing chemical for a bathroom?

No single product does the whole job. A flexible coating does most of the work: Hi-Flex or Seep Blocker 2K, two coats in the sunk and two under the tiles. WP+200 goes into the concrete and screed at 200 ml per 50 kg bag, and Seal & Dry SBR goes into the mortar for the gola and pipe sleeves. How carefully the work is done matters more than the brand.

Which areas of a bathroom need waterproofing?

The whole floor, twice. At least 1 ft up every wall: Dr. Fixit says 20 cm, Birla White at least 300 mm, and we use the higher figure. The wall you bathe at goes to about 4 ft with a bucket, or to the shower head with a shower. Every pipe through the floor, the floor trap, and the strip under the door frame need it too.

How is the sunken slab waterproofed?

Plumbing finished and tested first. Then pack every pipe sleeve with SBR mortar, make a rounded gola in every corner, and water-test the bare slab for 48 hours. Apply two coats of Hi-Flex or Seep Blocker 2K over the floor and sides, cure them, and water-test again with 50 mm of water for 48 hours. Protect the coat with a thin plaster before filling. Steps 1 to 9 above.

How long before we can use the bathroom? (bathroom kitne din baad use kar sakte hain)

About four weeks from a bare sunk to the first bath, done by the makers' sheets. Curing, two 48-hour water tests and a 7-day cure of the protection plaster take most of that. You can walk on the tiles 24 hours after laying them with TileStix.

Is WP+200 in the slab enough on its own?

No. WP+200 makes the concrete itself resist water, but bathroom leaks come through the gaps: round pipes, at the trap, at the floor-wall joint and through cracks. UltraTech's own brochure puts bathrooms among the places that need a coating on top as well.

Can it be done without breaking the tiles?

Sometimes. If water gets in only at open joints and round the trap, re-grouting with TileLynk and resetting the trap in SBR mortar can stop it. Dr. Fixit warns that re-grouting alone is unlikely to stop an existing leak, so check the ceiling below again after two weeks. If the stain stays, the floor sounds hollow or a pipe in the sunk is broken, the floor has to come up. Start with the 2-day test above.

Is the kitchen done the same way?

Yes, with the same products. Dr. Fixit notes that a kitchen usually has less standing water, so the treatment can be lighter. Corners, pipe openings and the sink wall up to counter height still need the coat. See kitchen waterproofing.

Will you come and check our bathroom?

We don't do site visits. Send us photos on WhatsApp at two points: before the sunk is filled (with the coat and the water test showing), and before the tiles go on. We'll look at them with you and say what we see.

Mr Mustafaa
Paint Engineer, Tashya Ventures

Paint Engineer at our Reva Road store, Muzaffarpur, where he handles paint, putty, tiles and waterproofing. Every figure on this page was checked against the maker's own sheet on 12 Nov 2026. Where the makers disagree, the page says so and gives the safer figure. Where a figure is local practice rather than a maker's, the page says "usual practice".

Where the numbers come from

  1. UltraTech, Weather Pro waterproofing brochure: WP+200 at 200 ml per 50 kg bag, added to half the water. Hi-Flex: powder and liquid mixed, 0.6–0.7 mm a coat, two coats at least 8 h apart and crosswise, 1 kg covers 14–15 sq ft (we read that as one coat), a screed or plaster on top recommended, up to 100% elongation, packs 12 and 24 kg. Bathrooms and kitchens are listed among the high-risk areas.
  2. Birla White, Seep Guard Seep Blocker 2K warranty booklet (3 kg pack): for bathroom, kitchen and sunken areas. Plumbing finished first, 28-day cure of new work, 50 × 50 mm gola in SBR polymer mortar with 3–4 days moist cure, 45 GSM glass mesh. Water tests at 50 mm for 48 h, before coating and 7 days after. Mix 2 parts powder to 1 part liquid with no water, 6–8 h between coats, 3–6 h air dry, 2–3 days moist cure, 3–4 days dry before submersion. Protection of 2–3 mm Levelplast or spatterdash (1:1:1.5) plus 12–15 mm 1:4 plaster, 7-day cure, screed at least 20 mm over pipes, no application above 35 °C surface. Warranty: 3 years, at least 12 kg on one surface, 7.5 sq ft per kg, registration within 30 days, no cover for leaks from traps, untreated tile joints or plumbing.
  3. Birla White, Seep Blocker 2K product page: up to 5 bar water pressure, up to 90% elongation, 3-year warranty.
  4. Birla White, Best method for bathroom waterproofing in Indian homes (23 Apr 2026): coat at least 300 mm up the walls and higher in the shower, two coats crosswise, 1–1.2 mm total, 5–6 h between coats.
  5. Birla White, How to waterproof an existing bathroom without major renovation: clean, remove loose tiles, repair cracks, two coats of Seep Blocker 2K over walls and floor.
  6. Dr. Fixit, Waterproofing FAQs: side walls to 20 cm, sunken slab coated and leak-tested before filling, re-grouting alone unlikely to stop an existing leak, kitchen treatment can be lighter, coat must be dry before the bathroom is used.
  7. Birla White, TileStix Intero Grip+ (TX2) and TileLynk product details: TX2 for ceramic tiles up to 450 × 450 mm indoors, walk after 24 h; TileLynk for joints of 1–6 mm.

Send us your bathroom size

Length, width and sunk depth. We'll send back the coating, WP+200, SBR and cement for it, with today's price, on WhatsApp.

TASHYABUILDING SOLUTIONS · MUZAFFARPUR
WhatsApp 90310 74624tashyaventures.com