हिंदी Call90310 74624
Home›Problems›Cracks
Problem · cracks in walls

Is this crack dangerous? Find out if it is still moving, and when to call an engineer

The short answer

A crack that has stopped is rarely dangerous. A crack that keeps growing is, whatever it looks like today. So the question is not only "what kind of crack is this" but "is it still moving", and a pencil and a strip of paper answer that in a month.

  • Call an engineer todaywider than 3 mm, wall bulging, a door that suddenly jams, or cracks in a beam, column or slab. The six signs
  • Anything else: watch it for 30 daysmark the ends, date it, glue a paper strip across. Don't fill it yet. The watch test
  • Stopped? Then it's the plaster's problemfill it with the right filler. Which filler for which crack
3 mm
Engineer firstAbout 4 ATM cards. The line UltraTech and Dr. Fixit both draw.
30 days
Shortest watchCheck weekly. Through a summer and a monsoon is better.
₹ 0
Cost of the testA pencil, a strip of paper, a little paste and your phone.
The watch test, set up on day 1
A wall crack marked for watching A diagonal crack in plaster. A pencil line and the date just past each end, two small pencil ticks where the width is measured, a paper strip glued across the crack, and a coin held beside it for the photo. 12 Nov12 Nov 0.5 mm 1 2 3 4
  • 1Pencil line just past each end, with the date. If the crack runs past it, it is growing longer.
  • 2Two ticks where you measure, so every reading is taken at the same spot.
  • 3Paper strip, paste only at its two ends. It tears if the crack opens.
  • 4A coin in every photo, so widths can be compared later.
Widths drawn larger than life. To read the width, use an ATM card or the printable card on our crack-types page.
Don't wait a month for these

Six signs that need an engineer today, not a watch test

With these, the house has already told you something is moving. Don't fill, don't paint, don't build further. Call.

1Wider than 3 mm

Four ATM cards held together slide in. UltraTech says cracks over 3 mm or growing fast need a professional check; Dr. Fixit puts its line at 3 mm too.

2The wall bulges, leans, or one side sits proud

Run your palm across the crack. If one edge stands out from the other, the wall has shifted, not just split.

3A door or window suddenly jams

A frame that closed last month and sticks now has been pushed out of square. Together with a new crack nearby, this is movement.

4A crack in a beam, column or slab

Especially along the line of a bar, or with brown rust stain coming out of it. These carry the house. Plaster cracks don't.

5The ceiling sags or pieces fall

Concrete falling from a slab, a ceiling you can see dipping, or many parallel cracks across it. Keep people out from under it.

6New cracks in several rooms at once

After a new floor was cast above, after a flood, or after a tremor. Many rooms at once points to the ground or the frame, not the plaster.

Until the engineer comes

  • Stop any building work above: no new dhalai, no stacking bricks, sand or sariya on the roof.
  • Don't fill a water tank on the roof to the brim if the cracks are in the slab or the top floor.
  • Keep people, especially children, away from a bulging wall or a sagging ceiling.
  • Mark and photograph every crack anyway (steps below). The engineer will want to know if they move.

Want to know what kind of crack it is from its place and shape (column joint, window corner, slab line, map cracks)? That is on our other page: is the crack in the plaster or the structure. This page is about time: whether it has stopped.

The watch test

Mark it, date it, and look again every week

Every crack we see falls into one of two stories: something happened once and stopped (the plaster dried, the house settled in its first years), or something is still happening. Only time tells the two apart.

  1. Pencil line past each endDraw a short line across the crack about a finger's width beyond each tip. Write the date beside it.
  2. Pick one spot and measurePut two small ticks on either side of the crack at its widest point. Read the width there with an ATM card (0.76 mm thick) or a printed crack card. Always measure at the same ticks.
  3. Glue a paper strip acrossA strip of thin paper, about two fingers wide. Paste only on its two ends, one each side of the crack, not on the middle.
  4. Photograph it with a coinHold a coin flat on the wall beside the crack, phone square to the wall. Same coin, same distance each time.
  5. Look every week for a monthSame time of day, because walls move with the heat. After the first month, look once a month.
  6. Write it downDate, width, strip whole or torn, past the line or not. Use the checker below, or a page in a notebook taped near the crack.

Best time to start is the day you find it. UltraTech advises looking at walls right after heavy rain or a hot spell, when cracks show most. Don't fill or paint a crack during the watch: it removes the evidence.

12 Nov 0.5 mm DAY 1

Day 1

You do: mark, date, strip, photo

Ten minutes. Write the first reading down.

12 Nov 0.5 mm DAY 30

A month later: steady

You see: nothing changed

Strip whole, crack short of both lines, same width. Keep one more check after the next hot or wet spell, then fill it.

12 Nov 1.5 mm ! DAY 30

A month later: moving

You see: past the line, strip torn, wider

Any one of these is enough. Stop, don't fill, and call an engineer with your notes and photos.

Reading the result

Steady, breathing or growing: three ways a crack behaves over a year

Walls swell in the wet and the heat and shrink back in the dry and the cold. So a crack that opens a little in May is not always a bad sign. What matters is whether it comes back.

Crack width over twelve months Width in millimetres from November to October. Steady: flat at about half a millimetre. Breathing: about one millimetre, wider in the summer and monsoon, back to one millimetre by October. Growing: rises step by step from under one millimetre and crosses the 3 mm line by the monsoon. SUMMERMONSOON 3 mm: ENGINEER 01234 mm NDJFMAMJJASO STEADYBREATHINGGROWING Width at the same two ticks, read once a month
An illustration of the three patterns, not readings from one house. Seasonal swelling and shrinking of building materials is one of the crack causes BIS SP 25 describes.
What your notes showWhat it means and what to do
Same width, strip whole, short of both linesFor 30 days or moreStopped
Plaster shrinkage or old settlement that has finished. Fill it: which filler for which crack.
Opens in heat or rain, closes againBack to the first width by winterBreathing
Heat or moisture movement, most often under a roof slab or along a wall-column joint. Fill with something that can move, not plain putty, and keep the roof cool and dry from above: terrace waterproofing.
Wider at each reading, or wider this summer than lastEven by half a millimetreGrowing
Something is still moving. Don't fill. Engineer, with your notes.
Ran past a pencil lineWidth may look the sameGrowing
Getting longer is growing too. Engineer.
Strip torn, but width reads the sameCards can't show small changesLook closer
Glue a new strip, check weekly for another month, and measure with a printed card. If the new strip tears too, treat it as growing.
Filled once, came back on the same lineAny widthMoving
Rigid filler can't hold a joint that moves. Watch it as above; if it grows, engineer, if it breathes, flexible filler with mesh.
Why "same time of day" mattersA wall in the afternoon sun is warmer and a crack in it can read a little different from the same crack at dawn. Measure at the same hour so you compare like with like. One odd reading is not a trend; two in a row is.
Check two readings

Put in your first and latest reading

It works out how fast the crack is changing and tells you which of the three it looks like. Then send the result to us or to your engineer.

First reading
Latest reading

An ATM card is 0.76 mm thick: one card ≈ 0.8 mm, two ≈ 1.5 mm, three ≈ 2.3 mm, four ≈ 3 mm.

What your readings say

——
Days between readings—
Change in width—
Rate—
Send these readings and photos on WhatsApp

This sorts your notes; it does not replace an engineer's eyes. The 3 mm line is UltraTech's and Dr. Fixit's. We treat any growth of half a millimetre or more as growth, because card readings can't be finer than that.

Houses around Muzaffarpur

Why our houses crack: a floor at a time, flood water, and a shaking ground

Most crack pages are written for flats built in one go. Here, a house usually grows over twenty years, stands on river soil, and sits in earthquake country. Each of those leaves its own cracks, at its own time.

Where a stage-built house cracks
A two-storey house with the top floor added later Ground floor built first, first floor added years later. Arrows show the new floor's weight going down old columns to old footings. Cracks show at the ground-floor beam and column joint, diagonally from a ground-floor window corner, and above the right footing where flood-soaked soil has settled. SOAKED SOIL BUILT FIRST ADDED LATER NEW WEIGHT ON OLD COLUMNS FLOOD WATER STOOD HERE 1 2 3 4
  • 1New floor's weight goes down columns and footings that may have been sized for one storey.
  • 2Crack at the beam-column joint on the ground floor, after the new dhalai.
  • 3Diagonal from a window corner, ground floor.
  • 4Diagonal over the corner that sank, where flood water soaked the soil.
A drawing of the pattern, not a design. Any of 2, 3 or 4 appearing in the months after a new floor or a flood is a reason for an engineer, even if narrow.

1A floor added years later

The ground floor goes up first; the family adds a floor when a son marries or money comes in. If the footings, columns and beams were sized for one storey, the new floor loads them beyond that. The cracks come within months of the new dhalai: at ground-floor beam-column joints, diagonally from ground-floor door and window corners, and in several rooms at once.

What to do: mark and date them the week they appear; if they grow, stop work above. Before you even plan the floor, read ground floor now, upper floor later.

2Flood-soaked soil

North Bihar's river soil carries a house well when it is evenly dry or evenly wet. After water stands round a house for weeks, one side can dry and settle more than the other. The cracks often show in the months after the water goes down, as the ground dries out: diagonal, over the corner that sank, sometimes with a plinth or floor that has dropped.

What to do: mark them now (October to January is exactly when they show) and watch through the dry season. Growing, or a corner floor sinking: engineer. See the house is settling on one side.

3A shaking ground

Muzaffarpur was badly damaged in the 1934 Bihar–Nepal earthquake, and the 1988 earthquake was felt across north Bihar. Even a small tremor can open old cracks or start new ones.

What to do: after any tremor you feel, walk round with your notes and compare every marked crack. New cracks in beams or columns: engineer.

4And the harmless one: hot-weather plaster

Fresh plaster in a Bihar May dries before it can set and shrinks into fine map-like cracks within weeks. These stop on their own. They are the reason most cracks on new houses are nothing to worry about.

If you are building now: keep new plaster wet for its full curing time and shade it from direct sun. That prevents this crack completely.

When to call, and who

The engineer: when to call, and what to show them

A shop can't tell you a wall is safe, and neither can a mason. A civil engineer who looks at the house, and at your notes, can. Here is how to make that visit count.

Call a civil or structural engineer when

  • Any of the six signs above.
  • The watch test shows growth: wider, longer, or the strip tore twice.
  • Cracks came after a new floor, a flood, a tremor, or digging next door.
  • A crack you filled has come back on the same line twice.
  • You plan to add a floor and there are cracks downstairs now.

Show them this

  • Your notes: dates, widths at the same ticks, strip torn or not.
  • The photos with the coin, in date order.
  • When the house was built, and when each floor was added.
  • The map or drawing, if there is one, and who built it.
  • How high flood water came, for how long, and when.
  • Any work since: new tank on the roof, borewell, digging or building next door.

Engineers who work in Muzaffarpur: our engineers list. Not sure yet? Send us photos on WhatsApp with a coin beside the crack, and we will look at them with you and tell you which kind it looks like. We don't make site visits for cracks, and we will never sell you a filler for a crack that needs an engineer.

Questions people ask us

Short answers

How do I know if a crack is growing? (crack badh raha hai kaise pata karein)

Draw a short pencil line just past each end of the crack and write the date beside it. Measure the width at one marked spot and glue a strip of paper across the crack. Look every week for a month. If the crack runs past a pencil line, the paper tears, or the width goes up, it is growing.

How long should I watch a crack before filling it?

At least 30 days, checking every week. Better still, through one summer and one monsoon, because some cracks open in the heat or the wet and close again. If nothing changes in that time, fill it.

A crack opens in summer and closes in winter. Is it dangerous?

Usually not. A crack that breathes with the seasons and comes back to the same width is heat or moisture movement, most often where a roof slab sits on a brick wall. It needs a filler that can move, not plain putty. A crack that is wider each summer than the last is growing, and needs an engineer.

Why did cracks appear after we built the first floor?

The new floor adds weight to columns, beams and footings that may have been sized for one storey. Cracks at beam-column joints, diagonal cracks from ground-floor window corners, or a door that starts sticking after the new dhalai all need an engineer before more work goes up. See ground floor now, upper floor later.

Cracks appeared after the flood. What should I do?

Mark and date them now, while the ground is still drying. Soaked soil can settle unevenly for weeks after the water goes. If they grow, if they appear in several rooms, or if a floor or plinth sinks at one corner, call an engineer.

How wide a crack needs an engineer?

Wider than 3 mm, about four ATM cards held together, as UltraTech and Dr. Fixit both say. Also any crack that is growing, whatever its width. UltraTech's same page also mentions 1 cm as the size for professional repair; we go by the safer 3 mm.

Is a hairline crack dangerous? (kya baal jaisa crack khatarnak hai)

Usually not, if it is in the plaster and stays the same. But a hairline in a beam, column or slab, or one that keeps getting longer, is watched like any other crack. Width tells you how bad it is now; growth tells you whether it is getting worse.

Can I fill the crack while I am watching it?

No. Filling or painting it hides the evidence, so you can no longer see whether it moves. Fill only after the watch shows it has stopped, or after an engineer has seen it.

Abhishek Ranjan
Diploma Civil Engineer, Tashya Ventures

Answers cement, steel and building questions at our Reva Road store, Muzaffarpur. The width lines on this page were checked against UltraTech's and Dr. Fixit's own pages on 12 Nov 2026. Where they differ, the page gives the safer figure.

Where the numbers come from

  1. UltraTech Cement, How to repair cracks in walls: hairline under 1 mm; over 3 mm or growing fast needs a professional check; over 1 cm get professional help; look after heavy rain or a hot spell; settlement cracks, watch if they widen.
  2. Dr. Fixit (Pidilite), Structural cracks vs surface cracks: under 1 mm usually surface; over 1 mm monitor; over 3 mm professional evaluation; tape across the crack, mark the ends, check monthly.
  3. Bureau of Indian Standards, SP 25:1984, Handbook on causes and prevention of cracks in buildings: non-structural cracks from moisture change, thermal movement, elastic deformation, creep, chemical reaction, foundation movement and vegetation.
  4. UltraTech, Weather Pro Hi-Flex coverage: 14–15 sq ft per kg for one coat (maker's figure).

Send us a photo of the crack

With a coin beside it, and your readings if you have them. We'll tell you which kind it looks like, on WhatsApp.

TASHYABUILDING SOLUTIONS · MUZAFFARPUR
WhatsApp 90310 74624tashyaventures.com