Mr Mustafaa, Paint Engineer · checked against the makers' sheets, 12 Nov 2026
The short answer
Catch the water
Clear the outlet
Find the entry point
Patch it in a dry spell
Fix it properly once the roof is dry
The wet patch on your ceiling is usually not under the hole: water runs inside the slab first. In rain, only a small cement and SBR patch is possible. No coating works on a roof that is getting rained on. The real job comes after: repair the cracks, fillet the parapet corner, two coats of Hi-Flex, and a screed on top.
8 h
Minimum gap between coatsHi-Flex goes on in two coats, the second laid crosswise. UltraTech.
~7
sq ft per kg, two coats1 kg covers 14–15 sq ft for each coat, so a finished job uses double.
1 ft
Up the parapetMost roof leaks start where the wall meets the slab. Carry the coating up it.
Why the drip is not under the hole
Not to scale. Water that gets into a crack runs along the slab before it finds a way down, so start the search on the roof, not on the ceiling.
While it is dripping
The first ten minutes
Three things, in this order. None of them needs a mistri.
1Make it safe
If water is near a light, fan, or switchboard, switch off that MCB (or the main switch) before you touch anything. Put a bucket under the drip and move the bed, cupboard and books. If the ceiling paint has ballooned with water, prick its lowest point over the bucket so it drains instead of spreading.
2Go up and let the water out
On the roof, pull the leaves and plastic out of the outlet and push the standing water towards it with a broom. This alone often stops the drip, because a crack only leaks hard while water stands over it. Take care on a wet roof, and stay off it in lightning.
3Take two photos
One of the ceiling stain and one of the roof directly above it, from the same corner of the house. They tell you, and us, where the water is getting in. Send them on WhatsApp 90310 74624.
On a flat roof, six places cause nearly every leak. The shape and position of the stain below tell you which one to check first.
Your roof from above
Stain on the ceiling
Check first
A band along the top of a wallOften the wall itself is damp at the top
1 · Parapet joint
In the corner under the outletWorse after heavy rain
2 · Outlet
A straight or zigzag lineLike a pencil mark across the ceiling
3 · Crack
A round patch that keeps growingKeeps dripping a day after the rain
4 · Low spot
Near the tank or a pipeCan drip even without rain
5 · Tank, sleeve
Many small patchesRoof coating chalky, cracked, flaking
6 · Old coating
Confirm it with a bucket of water, once the rain stops.
Pour water on one suspect spot at a time, keep it wet for up to an hour, and have someone watch the ceiling. Start at the parapet joint nearest the stain and work inwards. When the stain darkens again, you have found it. Mark the spot with chalk for the repair.
Stopping it in the rain
What holds until the weather clears, and what wastes your money
In a monsoon, you can only patch. A good patch on the right spot often holds for weeks. Do it in a break between showers.
The rain patch, in four steps
Mix ratios for the slurry and the mortar are printed on the Seal & Dry SBR pack. Use those, not another brand's. Add no extra water: the latex is the liquid.
✓Works for now
Clearing the outlet and sweeping water off. Free, and often enough to stop the drip.
A cement + Seal & Dry SBR patch pressed into a crack you have cut into a V, on a surface that is damp but has no water standing on it.
A tarpaulin laid so water runs off it towards the outlet, weighted at the edges. It must shed water, not hold a pool.
A patch is first aid. It does not replace the job below. Mark every patched spot so it gets repaired properly later.
✕Does not work
Any roof coating in the rain. Hi-Flex needs two coats 8 hours apart. Rain on a fresh coat washes it off, and the money goes with it.
Paint or putty on the ceiling inside. The stain comes back with the next rain, and the wet putty swells and falls.
Petrol mixed with thermocol. A fire risk on the roof, and it cracks in the sun within weeks.
Tar or plastic poured over standing water. It cannot stick to a wet surface, and plastic sheet held down by bricks traps a pool underneath.
After the rain
The proper fix, once the roof is dry
Wait for a few days of sun so the roof is dry to the touch and even in colour. Then do the whole roof in this order, not just the spot that leaked: water moves to the next weakest point. The full method is on the terrace waterproofing page.
The finished roof edge
Not to scale: the two coats are about 0.6–0.7 mm each. Coats, gap and screed: UltraTech Weather Pro brochure. Fillet and 1 ft upturn: usual practice.
Clean the whole roofSweep, scrape off loose old coating and moss, and clear the outlet and its pipe. A coating only grips a sound, clean surface.
Repair every crack and the rain patchesOpen each crack into a V, brush out the dust, and fill it with cement mortar made with WP+200 (200 ml per 50 kg bag of cement, added to the second half of the mixing water, as UltraTech says). Keep it damp for a few days. Moving cracks: joints and cracks.
Round the parapet cornerMake a cement-sand fillet, usually 2–3 inches, where the parapet meets the slab, so the coating does not have to bend round a sharp corner. Details: parapet waterproofing.
Fill the low spotsBuild up any spot where water stood with mortar, so all water runs to the outlet. Pack the gap around pipe sleeves and the tank base with SBR mortar.
Two coats of Hi-FlexMix the powder and liquid of Hi-Flex and lay the first coat over the roof, the fillet and 1 ft up the parapet. Wait at least 8 hours, then lay the second coat at right angles to the first. Prepare the surface and mix exactly as the pack says.
Screed on topUltraTech "highly recommends" a layer of screed or plaster over the coating. It protects it from feet, sun and the water tank's weight. Give it a slope to the outlet.
Pick the weather, not the date.
Start only on a day with no rain expected, so the first coat has its 8 hours and the second can follow. In Muzaffarpur the safe window is the dry months, and the best time is March to May, before the monsoon. Not leaking now? Our pre-monsoon roof check walks you round the roof in April.
How much for your roof
Hi-Flex for your roof, in packs
Put in the roof size inside the parapet. We count two coats, plus 1 ft up the parapet all round.
Your list
UltraTech Weather Pro Hi-Flex, 2 coats—1 kg covers 14–15 sq ft at 0.6–0.7 mm a coat (UltraTech). Two coats take double.—
Weather Pro WP+200, in the crack mortar200 mlper 50 kg bag of cement used for repairs and screed (UltraTech)Packs: 200 ml, 1 L, 5 L · Ask rate
Prices are from our latest bill and change often. Please confirm today's rate on WhatsApp or call before buying.
Seal & Dry SBR, patches and sleeves1 kgenough for a few cracks, the outlet and pipe sleeves on a house roofAsk today's rate
Searching for Dr. Fixit Roofseal?
You want a coating that covers the whole roof and bridges fine cracks. The one we keep for that is UltraTech Weather Pro Hi-Flex: by UltraTech's figures it stretches up to 100% and holds back water pressure up to 7 bar. Birla White Seep Blocker 2K (two-part, white cement with acrylic polymer, up to 5 bar, 3-year warranty by Birla White) is our small-pack choice for one spot. Which suits your roof: Hi-Flex vs Seep Blocker 2K. If you want Dr. Fixit itself, we can order it for you; ask on WhatsApp for the time it takes.
Chhat se pani tapak raha hai to sabse pehle kya kare?
Switch off the circuit if water is near a light, fan or switchboard. Put a bucket under the drip and move the bed and cupboard. Take a photo of the stain. Then go up, clear the outlet and push standing water towards it. Only after that, look for where the water gets in.
Can a roof be waterproofed in the rain, or while it is wet?
No. Hi-Flex goes on in two coats at least 8 hours apart, and rain on a fresh coat ruins it. In a break in the rain you can only patch: cut the crack into a V, brush a cement and SBR slurry on the damp (not flooded) surface and press in a stiff cement and SBR mortar. The coating waits until the roof has dried.
Chhat se pani tapakna kaise roke, hamesha ke liye?
Clean the roof, fill every crack with WP+200 mortar, fillet the parapet corner, fill the low spots, then two coats of Hi-Flex crosswise, at least 8 hours apart and 1 ft up the parapet, and a screed on top. The steps are above and on the terrace page.
Dr. Fixit Roofseal ki jagah kya lagaye?
For a whole roof, UltraTech Weather Pro Hi-Flex, which we stock. For one spot such as a tank base, Birla White Seep Blocker 2K. If you want Dr. Fixit itself, we can order it for you.
How much Hi-Flex for a 1000 sq ft roof?
UltraTech says 1 kg covers 14–15 sq ft at 0.6–0.7 mm a coat, and asks for two coats. So 1000 sq ft takes about 134–143 kg: six 24 kg packs, plus a little more for the parapet. Use the calculator above for your roof.
Will the patch I did in the rain last?
Weeks, sometimes a season, if it is on the right spot. It is first aid. Mark it, and include it in the proper repair once the roof is dry.
When can I paint the stained ceiling inside?
Only after the roof is fixed and the ceiling has dried fully. Test by touch and colour; it is usually a few weeks after the leak is stopped. Then see painting a wall that was damp.
The water comes in even when it has not rained. Why?
Then it is not the roof. Look at the water tank and its pipes, or a bathroom on the floor above: bathroom water in the room below.
Mr Mustafaa
Paint Engineer, Tashya Ventures
Paint Engineer at our Reva Road store, Muzaffarpur, and our waterproofing advisor. Every number on this page was checked against the maker's own published sheet on 12 Nov 2026. Where a figure is our usual practice rather than a maker's, the page says so.
Where the numbers come from
UltraTech, Weather Pro waterproofing brochure: Hi-Flex for terraces and roofs, 0.6–0.7 mm per coat, two coats at least 8 hours apart with the second perpendicular, screed or plaster "highly recommended" on top, 1 kg covers 14–15 sq ft, elongation up to 100%, up to 7 bar, packs 12 and 24 kg. WP+200: 200 ml per 50 kg bag of cement, added to the second 50% of the water.
Birla White, Seep Blocker 2K page: two-part coating of white cement, silica sand and acrylic polymer, up to 5 bar, elongation up to 90%, 3-year warranty.
UltraTech Seal & Dry SBR pack: mix ratios for slurry and repair mortar. We print no ratios from other brands' SBR.
Coverage per coat: UltraTech gives 14–15 sq ft per kg next to a 0.6–0.7 mm coat. A kilo of mix cannot spread two coats of that thickness over 14 sq ft, so we count the figure per coat and double it for the job. That way you do not run short halfway.
Send us a photo of the stain and the roof
We will tell you where the water is most likely getting in and what to buy, with today's price, on WhatsApp.